Y. Liu,H.D. Liu,Vasiliy Pelenovich,Qiang Wan,J.L. Guo,Y.M. Chen,Jun Zhang,Longjian Xue,Zhihang Li,Bing Yang
出处
期刊:Vacuum
[Elsevier BV]
日期:2021-08-11
卷期号:193: 110516-110516
被引量:51
标识
DOI:10.1016/j.vacuum.2021.110516
摘要
Fabricating a multilayer structure with different modulation periods (Λ) is an attractive approach to adjust the properties of the monolithic coatings. Here, multi-layered AlTiSiN/AlCrSiN coatings with Λ ranging from 25 to 147 nm were prepared by the arc ion plating technique. The effects of Λ on the structure and properties of the coatings were investigated systematically. Results showed that all the coatings had a mixed-phase structure consisting of TiN and CrN in rock salt structure and AlN in wurtzite structure. The coating at Λ = 60 nm displayed the optimized hardness and elastic modulus, corresponding to 31.6 GPa and 514 GPa, and the coating at Λ = 25 nm possessed the highest adhesion strength with L c1 = 41.5 N, L c2 = 80.2 N, and CPR S = 1606.1 N 2 . The tribological test showed that the AlTiSiN/AlCrSiN coatings exhibited abrasive wear behavior and the coating at Λ = 25 nm demonstrated the lowest COF of 0.26 and the minimum wear rate of 8.3 × 10 −7 mm 3 /Nm. • AlTiSiN/AlCrSiN multilayer coatings with various modulation period ranging from 25 to 147 nm were prepared by arc ion plating. • Properties of the AlTiSiN/AlCrSiN coatings were significantly affected by the modulation period. • The coating with Λ = 60 nm displayed the maximum hardness of 31.6 Gpa and elastic modulus of 514 GPa. • The coating with Λ = 25 nm demonstrated the highest adhesion strength of and the best wear resistance.
科研通智能强力驱动
Strongly Powered by AbleSci AI