Electrolytic hydrogenation and post-solution heat treatment was repeated to refine the coarse β-transformed grain structure of Ti-6Al-4V (Ti- 64) and Ti-4.5Al-3V-2Mo-2Fe (SP700) alloys. The sheet specimens with 2mm β-transformed grains were hydrogenated at 100 mA/cm^2 for 2h and then at 10 mA/cm^2 for 2h in 1N H_2SO_(4(aq)) by adding 0.1g/ L As_2O_3, and then subjected to a thermal solution treatment at 300 ℃ for 2h in a muffle furnace. The treatment was repeated 4 times with the last treatment at 450 ℃ for 2h. The specimens with coarse grains (2mm) were refined to 10μm. The micro-hardness of Ti-64 and SP700 was enhanced by 70% and 54%, respectively.