Jaemin Son,Hwon Park,Min-Ju Kim,Jae Hui Park,Ki‐Ho Nam,Jin-Seok Bae
出处
期刊:Polymers
[Multidisciplinary Digital Publishing Institute]
日期:2024-06-16
卷期号:16 (12): 1716-1716
被引量:10
标识
DOI:10.3390/polym16121716
摘要
Polymers with a low dielectric constant (Dk) are promising materials for high-speed communication networks, which demand exceptional thermal stability, ultralow Dk and dissipation factor, and minimum moisture absorption. In this paper, we prepared a series of novel low-Dk polyimide films containing an MCM-41-type amino-functionalized mesoporous silica (AMS) via in situ polymerization and subsequent thermal imidization and investigated their morphologies, thermal properties, frequency-dependent dielectric behaviors, and water permeabilities. Incorporating 6 wt.% AMS reduced the Dk at 1 MHz from 2.91 of the pristine fluorinated polyimide (FPI) to 2.67 of the AMS-grafted FPI (FPI-g-AMS), attributed to the free volume and low polarizability of fluorine moieties in the backbone and the incorporation of air voids within the mesoporous AMS particles. The FPI-g-AMS films presented a stable dissipation factor across a wide frequency range. Introducing a silane coupling agent increased the hydrophobicity of AMS surfaces, which inhibited the approaching of the water molecules, avoiding the hydrolysis of Si–O–Si bonds of the AMS pore walls. The increased tortuosity caused by the AMS particles also reduced water permeability. All the FPI-g-AMS films displayed excellent thermooxidative/thermomechanical stability, including a high 5% weight loss temperature (>531 °C), char residue at 800 °C (>51%), and glass transition temperature (>300 °C).
科研通智能强力驱动
Strongly Powered by AbleSci AI