ABSTRACT PA6/polypropylene (PP) blends are investigated for obtaining balanced strength and toughness. The focus of this study is to understand the effect of PP content on mechanical property, water absorption, impact strength, thermal behavior, and morphology of PP in the absence and presence of PP‐ g ‐maleic anhydride compatibilizer. In comparison to pure PA6, all blends have higher impact strength with 161 and 124% increase at 5 wt % PP content in uncompatibilized and compatibilized blends (UB and CB), respectively. Morphology of impact fractured samples shows brittle fracture in the case of CB. scanning electron microscope of cryogenically fractured samples show decrease in domain size and change in shape from ellipsoid to spherical, from UB to CB. Then, 75% reduction in water absorption is observed for 50 wt % PP content UB. Postwater absorption yield strength (YS) remains constant above 10 wt % PP in both UB and CB and decrease in YS is less at higher PP content in CB. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2019 , 136 , 47690.
科研通智能强力驱动
Strongly Powered by AbleSci AI