A kind of the materials for the bipolar plate of proton-exchange membrane fuel cells(PEMFC) were fabricated by the hot-pressure molding with graphite powders and phenol-formaldehyde(PF) resin powders.The factors including the PF resin content,the graphite particle size and curing temperature which affected the conductivity and bending strength of the composite were investigated.The results showed that the conductivity decreased and bending strength increased with the increasing of PF resin content,that the conductivity and bending strength would increase firstly and then decreased with the increasing of graphite particle size,and that the conductivity surged greatly and bending strength would increase firstly and then decrease with the increasing of curing temperature,that the electrical conductivity and bending strength of the composite were 142 S/cm,61.6 MPa,when the PF resin mass content,graphite particle size and curving temperature were 15%,105 μm and 240℃.