印刷电路板
铜
杂质
材料科学
离子
船上
冶金
化学
电气工程
工程类
航空航天工程
有机化学
作者
Xianming Chen,Wei He,Benxia Huang,Hongbin Cui,Weibin Zhou,Kaijian Cai,Wanjin Wang,Guoqin Chen,Shouxu Wang,Yuanming Chen
标识
DOI:10.1080/00202967.2025.2517442
摘要
Some potential impurities could be found in copper plating solution with the utilisation of insoluble anodes and the addition of CuO. The influences of Fe2+/Fe3+ redox couple, NH4+ and Ti4+ on the performance of copper electrodeposition were investigated. The mechanism of Fe3+/Fe2+ in the plating solution was investigated to determine the impact of the ferric/ferrous (Fe3+/Fe2+) redox couple on the behaviour of polyethylene glycol (PEG) and bis-(3-sulphopropyl) disulphide (SPS) during copper electrodeposition. Experimental results showed that the thickness of the copper layer was inhibited but the throwing power was improved in the presence of the Fe2+/Fe3+ redox couple while current efficiency was diminished. However, little significant difference was obtained in the throwing power, current efficiency, morphology and thermal stress with Ti4 + and NH4+ in the plating solution.
科研通智能强力驱动
Strongly Powered by AbleSci AI