Newell H. Moser,Zachary Norris Buck,Nicholas A. Derimow,May L. Martin,Damian S. Lauria,Enrico Lucon,Peter E. Bradley,Matthew Connolly
出处
期刊:ASME 2010 Pressure Vessels and Piping Conference: Volume 6, Parts A and B
日期:2024-07-28
被引量:2
标识
DOI:10.1115/pvp2024-122545
摘要
Abstract Hydrogen is known to deteriorate the mechanical performance of steels (i.e., hydrogen embrittlement). The welding processes involved in the manufacturing and joining of steel pipelines locally modifies the microstructure of the steel, further complicating the situation. NIST has evaluated three steel pipes from industrial contacts to assess the susceptibility of seam welds to hydrogen embrittlement; these three pipes are made from API 5L X65M steel. The three steels were characterized in terms of microstructure, Charpy experiments (performed in air), and fracture toughness via single-edge notched bend specimens (performed in pressurized hydrogen). When testing in air, there was an apparent reduction in toughness for welded regions relative to the baseline steel. In hydrogen, a significant reduction in toughness was observed, however, the welded regions were the toughest. Microstructural differences in the welded region, namely grain size and the presence of phases like bainite, likely have the largest influence on these toughness differences.
科研通智能强力驱动
Strongly Powered by AbleSci AI