Abstract The dielectric behavior of amine‐terminated butadiene acrylonitrile rubber/DGEBA epoxy resin bleuds of different formulations has been studied in the temperature range −120–160°C at 10kHz. As indicated by the constancy of the glass transition temperatures of the two components, the degree of segmental mixing was very low or nil, irrespective of cure schedules. The intensity of the α‐relaxation of the rubber was much less than that predicted by the simple series model (lower bound). This has been attributed to incomplete phase separation at gelation. Measurements carried out with a nonreactive rubber support this conclusion. Part of the rubber remains molecularly dispersed within the glassy matrix, thus contributing to the modification of the mechanical properties of epoxy resins brought about by reactive rubbers.