摘要
Dissolved V in austenite of 7%Cr-0.4%V-0.09%N steel (hereinafter, % means mass%) was measured and the solubility product of VN was determined as follows:log([%V][%N]) = 4.38−(8436/T)where T is the absolute temperature in K. The solubility product obtained is 3 to 5 times larger than those in the literature and about one order larger than that for iron. The decrease in the activity coefficient of nitrogen due to the presence of Cr and V in the experimental steel is responsible for the increase in the solubility product of VN.