Anand Mohan P,Sreelakshmi Jayaprakash,Mariya George,Toto Sudiro,Oman Zuas,Tushar H. Rana,Nanda Kumar Amal Kaitheri
摘要
Rapid synthesis of the layered compound, lithium chromium (III) oxide (LiCrO 2 )—belonging to the alpha‐sodium iron (III) oxide (α‐NaFeO 2 ) structural family ( R m space group)—via the reactive flash (RF) method, is reported for the first time, achieving complete phase formation at a furnace temperature of ∼260°C within just 2.5 min. A secondary Li‐excess phase, identified as lithium chromium (VI) oxide (Li 2 CrO 4 ), is observed alongside the primary layered phase which is readily removed through aqueous washing followed by drying. Based on observational evidence and region‐specific microstructural and spectroscopic analyses, both chemical reactions (owing to the temperature surge) and probable electrochemical reactions (from the electric field close to the electrodes) of the RF process are identified. While the major phase along the gauge length lies in the proximity of the LiCrO 2 terminal phase, close to the electrodes, it is on the LiCrO 2 –Li 2 CrO 4 binary or LiCrO 2 –Li 2 CrO 4 –Cr 2 O 3 ternary phase fields. Defect equilibria, evaluated using the Brouwer approximation, suggest that Li‐vacancies and accompanying electronic (hole) carriers may dominate electrical conductivity via grains between 30°C–400°C under ambient oxygen partial pressures, with an activation energy of ∼0.14 eV. At elevated temperatures, Li‐ion migration through vacancies becomes increasingly likely. The activation energy for grain boundary conduction is nearly twice that of grain (bulk) conduction, indicating significant microstructural influence on overall transport behavior.
科研通智能强力驱动
Strongly Powered by AbleSci AI