材料科学
高熵合金
层错能
延展性(地球科学)
极限抗拉强度
材料的强化机理
叠加断层
应变硬化指数
位错
冶金
复合材料
合金
蠕动
作者
Daixiu Wei,Wu Gong,Tomohito Tsuru,Ivan P. Lobzenko,Xiaoqing Li,Stefanus Harjo,Takuro Kawasaki,Hyeon-Seok Do,Jae Wung Bae,Christian Wagner,Guillaume Laplanche,Yuichiro Koizumi,Hiroki Adachi,Kenta Aoyagi,Akihiko Chiba,Byeong‐Joo Lee,Hyoung Seop Kim,Hidemi Kato
标识
DOI:10.1016/j.ijplas.2022.103443
摘要
Face-centered cubic single-phase high-entropy alloys (HEAs) containing multi-principal transition metals have attracted significant attention, exhibiting an unprecedented combination of strength and ductility owing to their low stacking fault energy (SFE) and large misfit parameter that creates severe local lattice distortion. Increasing both strength and ductility further is challenging. In the present study, we demonstrate via meticulous experiments that the CoCrFeNi HEA with the addition of the substitutional metalloid Si can retain a single-phase FCC structure while its yield strength (up to 65%), ultimate strength (up to 34%), and ductility (up to 15%) are simultaneously increased, owing to a synthetical effect of the enhanced solid solution strengthening and a reduced SFE. The dislocation behaviors and plastic deformation mechanisms were tuned by the addition of Si, which improves the strain hardening and tensile ductility. The present study provides new strategies for enhancing HEA performance by targeted metalloid additions.
科研通智能强力驱动
Strongly Powered by AbleSci AI