The YK 1 shipwreck, found at Yenikapı, Istanbul, is one of 37 shipwrecks dating to the medieval era. This paper describes the studies and the processes which were conducted to conserve the YK 1. Firstly, the level of physical and chemical degradation of the wood from the YK 1 was examined, which revealed that the wood was highly degraded. Therefore, PEG 2000 was chosen for the impregnation process before vacuum freeze-drying. In addition, the ASE values confirmed that the PEG 2000 impregnation and vacuum freeze-drying method together were successful in conserving the YK 1, with values higher than PEG 2000 impregnation and vacuum freeze-drying methods alone. The concentration of the PEG solution in the tank was monitored throughout the impregnation process. Following this, samples taken from the wood cores were analysed using FTIR to evaluate the effectiveness of the impregnation process. Finally, SEM was used to examine the effectiveness of the PEG 2000 impregnation and vacuum freeze-drying method. The SEM images showed that the PEG 2000 was uniformly distributed, and the wood had no deformation after freeze-drying.
科研通智能强力驱动
Strongly Powered by AbleSci AI