Liquid slag tapping cyclone combustion technology under oxy-fuel conditions is a viable approach to resolve the combustion issues related to high-alkali coal. However, the impact of ash composition on slag flow behaviors under oxy-fuel conditions remains insufficiently understood. In this study, the synthetic ash was formulated with various oxide reagents based on the statistical data of Zhundong coal, and the influence of each ash composition on high-temperature flow behaviors under oxy-fuel conditions was systematically investigated. Under the conditions of holding at 1300°C for 15 min, Na2O tends to enhance flow characteristics, with flow length and area increasing from 13.35 mm and 181.26 mm2 to 60.00 mm and 1121.06 mm2 as Na2O rises from 5% to 13%. The CaO within the range of 2–24% promotes flow, but an excessively high CaO content negatively impacts flow characteristics. The MgO adversely affects flowability within the range of 4%–12%, where both flow length and flow area decrease as the MgO content increases. The flow characteristic exhibits a tendency to increase and then decline with a rise in Fe2O3 content. The slag with 35% SiO2 is partially molten with the best flow characteristics in the experimental conditions. When the SiO2 content increases to 73%, slag melts more completely, while the viscosity increases, leading to a decline in flow characteristics. With the increasing Al2O3 content, the flow length fluctuates. This study contributes to the safe and clean combustion of high-alkali coal and secure operation of boilers.