Li₂NiO₂ (LNO) is a promising cathode-side prelithiation additive for compensating irreversible Li + loss in lithium-ion batteries, but its practical use is hindered by sluggish Li + release and high sensitivity to ambient H₂O and CO₂. Herein, Na-modified Li₂NiO₂ was prepared by a sodium-acetate-assisted post-treatment, which introduces Na into the material and is associated with an acetate-derived carbon-containing surface region. Among the tested nominal Na/Li precursor ratios (1–3 mol%), LNO-2 (2 mol%) delivers the highest first-charge capacity of 451.3 mAh g −1 at 0.1C, exceeding pristine LNO by 126.5 mAh g −1 . On compressed powder pellets, the apparent water contact angle increases from 73.1° to 132.4°, while the total residual alkali content after 2 days of identical ambient-air exposure decreases from 1.22 to 0.42 wt%. After the same exposure treatment, LNO-2 also shows a smaller impedance response than pristine LNO. Incorporating 5 wt% LNO-2 into NCM811 cathodes increases the first discharge capacity from 205.9 to 240.9 mAh g −1 and the initial Coulombic efficiency from 80.5% to 87.7%. In NCM811||graphite full cells, LNO-2 increases the initial discharge capacity and the capacity retention after 100 cycles. These results show that sodium-acetate-assisted Na modification and surface modification improve the electrochemical usability and air tolerance of LNO-based cathode prelithiation additives. The present data, however, do not resolve a specific crystallographic Na site or quantitatively separate the contributions of Na modification and the carbon-containing surface species.
科研通智能强力驱动
Strongly Powered by AbleSci AI