Matthias Hahn,Hilmi Buqa,Patrick Ruch,Dietrich Goers,Michael E. Spahr,Joachim Ufheil,Petr Novák,R. Kötz
出处
期刊:Electrochemical and Solid State Letters
[The Electrochemical Society]
日期:2008-01-01
卷期号:11 (9): A151-A151
被引量:94
摘要
The thickness change of porous multiparticle graphite electrodes upon first electrochemical lithium intercalation and extraction was investigated by means of electrochemical dilatometry. For all investigated graphites, expansion starts well above 0.5 V vs and thus, before any unsolvated Li intercalation compounds are formed. This finding can be explained by solvent co intercalation during the first charge prior to SEI formation, as described by the Besenhard model. At potentials vs , i.e., in the region of unsolvated intercalation, the dilatation curves reveal the same major staging features that are seen in the corresponding potential profiles.
科研通智能强力驱动
Strongly Powered by AbleSci AI