Huajing Zong,Nan Kang,Mohamed El Mansori
出处
期刊:Wear
[Elsevier BV]
日期:2025-02-04
卷期号:571: 205859-205859
被引量:9
标识
DOI:10.1016/j.wear.2025.205859
摘要
The laser powder bed fusion (LPBF) process can produce H13 steel with a relative density exceeding 99.9 % by preheating the substrate. The mechanical properties of the alloy can be further enhanced through heat treatment (HT). This work investigated the microstructure and wear behavior of LPBF-processed H13 steel preheated at 500 °C (PT500H13) after HT. The sample tempered at 500 °C for 8 h (H13-500/8h) exhibited a hardness of 678.95 ± 11.14 HV1.0, and the cellular structure was still retained. After tempering at 550 °C for 4 h (H13-550/4h), the hardness increased to 664.77 ± 13.06 HV1.0, with a dissolved cellular structure. The wear resistance of H13-550/4h was superior to that of H13-500/8h, and both materials significantly outperformed conventionally manufactured H13 steel (CM-H13). Under a low applied load, the H13-550/4h and H13-500/8h steels were more prone to oxidation than CM-H13 was, leading to the formation of a tribo-oxide layer (TOL) that reduced the coefficient of friction (COF) and wear rate. H13-500/8h entered the oxidative wear stage earlier than H13-550/4h did, probably because of the high number of fine carbides. Compared with that in H13-550/4h, the cellular structure in H13-500/8h effectively hindered crack propagation into the substrate, resulting in a lower degree of delamination wear. The primary wear mechanisms for H13-500/8h were oxidative wear and abrasive wear, whereas material loss for H13-550/4h was attributed mainly to oxidative wear and delamination wear. The wear mechanism of CM-H13 transitioned from delamination wear under a low applied load to delamination wear, oxidative wear, and abrasive wear under a high applied load.
科研通智能强力驱动
Strongly Powered by AbleSci AI