材料科学
复合材料
刮擦
断裂韧性
相对密度
陶瓷
烧结
复合数
压痕硬度
热压
微观结构
多孔性
韧性
粒度
陶瓷基复合材料
相(物质)
热等静压
钛
兴奋剂
抗弯强度
增韧
作者
Chandra Obulesu Bapanapalle,Ruchika Dhyani,Nitin Mahato,Soumyadip De,Nilrudra Mandal
摘要
ABSTRACT Zirconia‐toughened alumina (ZTA) ceramics reinforced with Ti 3 AlC 2 MAX phase are successfully fabricated through pressureless sintering to investigate the influence of Ti 3 AlC 2 addition on the microstructural, physico‐mechanical properties and scratch resistance behavior of the composites. Ti 3 AlC 2 content varies from 0 to 5 wt.%, and the green compacts are prepared by uniaxial pressing at 200 MPa followed by sintering at 1350°C under an argon atmosphere. XRD analysis confirms the successful retention of Ti 3 AlC 2 within the ZTA matrix without the formation of secondary phases. The monolithic ZTA exhibits a density and relative density of 4.12 g/cm 3 and 96.17%, respectively, which increases to a maximum of 4.14 g/cm 3 and 96.68% at 2 wt.% Ti 3 AlC 2 addition. FESEM analysis reveals significant grain refinement at lower reinforcement contents. The microhardness increases from 1736 HV for monolithic ZTA to 1938 HV at 2 wt.% Ti 3 AlC 2 , while fracture toughness improves from 4.45 to 5.54 MPa.m 0.5 due to crack deflection, crack bridging and crack branching mechanisms induced by the layered Ti 3 AlC 2 structure. Furthermore, the 2 wt.% Ti 3 AlC 2 composite exhibits superior scratch resistance with the minimum scratch depth among all compositions.
科研通智能强力驱动
Strongly Powered by AbleSci AI