氢脆
材料科学
脆化
氢
延展性(地球科学)
层错能
冶金
环境应力断裂
氧化物
微观结构
蠕动
腐蚀
化学
有机化学
作者
Motomichi Koyama,Eiji Akiyama,Young‐Kook Lee,Dierk Raabe,Kaneaki Tsuzaki
标识
DOI:10.1016/j.ijhydene.2017.02.214
摘要
Hydrogen and fuels derived from it will serve as the energy carriers of the future. The associated rapidly growing demand for hydrogen energy-related infrastructure materials has stimulated multiple engineering and scientific studies on the hydrogen embrittlement resistance of various groups of high performance alloys. Among these, high-Mn steels have received special attention owing to their excellent strength – ductility – cost relationship. However, hydrogen-induced delayed fracture has been reported to occur in deep-drawn cup specimens of some of these alloys. Driven by this challenge we present here an overview of the hydrogen embrittlement research carried out on high-Mn steels. The hydrogen embrittlement susceptibility of high-Mn steels is particularly sensitive to their chemical composition since the various alloying elements simultaneously affect the material's stacking fault energy, phase stability, hydrogen uptake behavior, surface oxide scales and interstitial diffusivity, all of which affect the hydrogen embrittlement susceptibility. Here, we discuss the contribution of each of these factors to the hydrogen embrittlement susceptibility of these steels and discuss pathways how certain embrittlement mechanisms can be hampered or even inhibited. Examples of positive effects of hydrogen on the tensile ductility are also introduced.
科研通智能强力驱动
Strongly Powered by AbleSci AI