摘要
Interfacial instability is a primary factor limiting the cycling durability of lithium metal batteries (LMBs), particularly for LIBs within solid polymer electrolytes (SPEs). Without interfacial solvent mediation, repeated lithium plating/stripping accelerates contact loss and the accumulation of interfacial damage, leading to impedance growth or soft short-circuit failure. Here, we report a self-healable semi-interpenetrating (semi-IPN) SPE that enables operando repair of electrochemically induced interfacial defects. The electrolyte is made with linear poly(ethylene oxide) (PEO) and a trifunctional furan/maleimide (TF/TMI) dynamic crosslinking scaffold based on reversible Diels–Alder (DA) chemistry to result in a dissociative covalent adaptable network-based semi-interpenetrating network. The resulting SPE sustains Li|SPE|Li cycling for 915 h at 0.2 mA cm−2 and 60 °C. Notably, electrochemical performance could be partially restored after soft short-circuit events by thermal activation of the dynamic network and by evidencing recovery of interfacial continuity. Moreover, full cells employing this functional SPE exhibit improved cycling stability (91.1% capacity retention after 350 cycles at 0.2 C) compared with those using conventional PEO electrolytes. This study demonstrates that the crosslinked dynamic covalent chemistry embedded in a linear polymer SPE platform can function as an interfacial repair mechanism, providing a practical strategy to manage inevitable interface degradation in LMBs.
科研通智能强力驱动
Strongly Powered by AbleSci AI