材料科学
纳米复合材料
天然橡胶
热稳定性
复合材料
碳纳米管
极限抗拉强度
固化(化学)
傅里叶变换红外光谱
抗撕裂性
化学工程
工程类
作者
Saowaroj Chuayjuljit,Piyaphorn Mungmeechai,Anyaporn Boonmahitthisud
标识
DOI:10.1177/0095244316639634
摘要
Epoxidized natural rubber (ENR)/multiwalled carbon nanotube (MWCNT) nanocomposites were prepared via in situ epoxidation of natural rubber (NR) using a molar ratio of formic acid/hydrogen peroxide to isoprene unit at 0.75/0.75 with five loadings of MWCNTs, ranging from 0.5–2.5 parts per hundred parts of rubber (phr), at 50°C for 4 h. Based on Fourier transform infrared spectra, the epoxide content of ENR in the nanocomposites was about 32.5–33.2 mole%. Accordingly, the products were referred to ENR30/MWCNT nanocomposites. The curing characteristics, mechanical properties (tensile properties, tear strength, and hardness), glass transition temperature ( T g ), thermal stability, and oil resistance of these in situ ENR30/MWCNT nanocomposites were investigated and compared with NR and neat ENR30. The results showed that the scorch and cure times of ENR30/MWCNT nanocomposites were the longest followed by NR and ENR30. The incorporation of an appropriate amount of MWCNTs into the in situ epoxidation apparently improved the properties of NR. Among them, the nanocomposites filled with 2 phr MWCNTs exhibited the highest mechanical properties, T g , thermal stability, and oil resistance. The mechanical properties of the in situ nanocomposites were also compared with those of the control nanocomposites prepared by adding MWCNTs directly in the prepared ENR30 latex. It was found that at similar MWCNT loadings, the in situ nanocomposites exhibited higher mechanical properties than the control nanocomposites.
科研通智能强力驱动
Strongly Powered by AbleSci AI