天然橡胶
尿素
十二烷基硫酸钠
蛋白水解酶
化学
氨
氮气
孵化
核化学
高分子化学
材料科学
色谱法
酶
有机化学
生物化学
作者
Warunee Klinklai,Takayuki Saito,Seiichi Kawahara,Kei Tashiro,Yasuyuki SUZUKI,Jitladda Tangpakdee Sakdapipanich,Yoshinobu Isono
摘要
Abstract Preparation of hyperdeproteinized natural rubber was made from fresh latex and preserved high‐ammonia latex by treatment with urea in the presence of sodium dodecyl sulfate. Concentration of urea, temperature, and time for the incubation were investigated to remove the proteins effectively. Under the best conditions, the total nitrogen content and amount of allergenic proteins for the deproteinized rubbers were 0.005 wt % and 1.0 μg/ml, respectively, which were less than those of natural rubber deproteinized with proteolytic enzyme. The hyper‐deproteinized natural rubber was proved through FT IR spectroscopy. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 555–559, 2004