DOI:10.1016/j.foodres.2024.113944
摘要
In this study, electrospun zein/alginate dialdehyde (AD) nanofibers were prepared by green crosslinking. The degree of crosslinking could reach 50.72 %, and the diameter of electrospun fibers ranged from 446.2 to 541.8 nm. The generation of AD and the bonding of crosslinking were further confirmed by the changes on characteristic peaks and conformational ratios in the infrared spectroscopy and secondary structure analysis. High concentrations of AD led to improved thermal stabilities, mechanical properties, and hydrophobicity. And the highly crosslinked nanofibers (Z-8) owned the highest elastic modulus (24.92 MPa), tensile strength (0.28 MPa), and elongation at break (8.14 %) among five samples. Moreover, Z-8 possessed a high swelling ratio of 5.45 g/g, and a low weight loss of 6.09 %. The samples could encapsulate curcumin efficiently and show controllable release behaviors based on different AD addition. And the oxidation resistance of nanofibers gradually improved, consistent with the release performances. This study indicated AD crosslinking favored the preparation and application of zein nanofibers, and the oxidized polysaccharide acted as the green crosslinking agent, which provided reference value for the application of polysaccharides in food-related electrospun materials.
科研通智能强力驱动
Strongly Powered by AbleSci AI