材料科学
金属间化合物
冶金
合金
极限抗拉强度
降水
粉末冶金
热机械加工
粒度
材料的强化机理
相(物质)
微观结构
沉淀硬化
产量(工程)
复合材料
固溶强化
晶界强化
晶界
烧结
基质(化学分析)
拉伸试验
固溶体
晶粒生长
机械强度
作者
Yucheng Zhou,Hu Cheng,Jiancheng Li,Meng Zhang,Pinqiang Dai,Tao Yang
标识
DOI:10.1177/02670836261494508
摘要
To overcome the low room-temperature strength of CoCrNi medium-entropy alloy (MEA) for structural applications, Mo was introduced via a powder metallurgy route, followed by cold rolling and subsequent annealing. Mo addition promotes the formation of σ (Cr-Mo) and μ (Co-Mo) intermetallic phases, with the σ phase exhibiting a cross-scale distribution at both submicron and micron levels. After thermomechanical processing, the precipitates become more uniformly dispersed, and the matrix grain size refines from 43.69 μm to 5.34 μm. Compared with the base alloy, yield strength increases from 405 ± 21 MPa to 755 ± 17 MPa and ultimate tensile strength from 823 ± 13 MPa to 957 ± 15 MPa, while maintaining 17 ± 2% total elongation. The strength improvement is due to precipitation, grain boundary, solid solution, and hetero-deformation-induced (HDI) strengthening.
科研通智能强力驱动
Strongly Powered by AbleSci AI