Abstract The structure of the oxide scales formed on three ferritic/martensitic (F/M) steels, including HT9, T91 and CLA16 exposed to oxygen-saturated lead-bismuth eutectic (LBE) at 400°C for 500 h has been studied. The results show that the oxide scales in the three steels have a similar triple-layered structure. The outer layer is a nanosized/ultrafine magnetite containing massive Pb solid solution nanoparticles. An Fe-Cr spinel constitutes the intermediate layer without the Pb particles. The innermost layer is a Cr oxide (i.e., Cr2O3) that forms preferentially at the martensite lath boundaries. A refined oxidation mechanism is proposed with consideration of the Cr oxide formed at the oxidation front, as well as of an improved “Pb nano-channels” theory.