材料科学
因瓦
微观结构
放电等离子烧结
复合材料
涂层
复合数
烧结
热膨胀
作者
Qiangqiang Nie,Bin Wang,Jianhua Zhang,Wenming Tang
标识
DOI:10.1016/j.matlet.2022.132440
摘要
• Ag(Invar) powder prepared by electroless plating Ag on the Invar powder. • The Ag(Invar)/Cu composites prepared by SPS at low temperature for a short time. • Effects of the Ag coating on microstructure and properties of the composites. • The 50Ag(Invar)/Cu composites have the highest TC of 151.6 W/(m·K). Cu matrix composites reinforced with 50 wt% Ag-coated Invar (Ag(Invar)) powder were prepared by spark plasma sintering at temperatures of 700 °C and 750 °C. Effects of the Ag coating and sintering temperature on microstructure and performance of the Ag(Invar)/Cu composites were studied. The results indicated that the Ag coating could promote densification of the composites, restrain the Invar/Cu interface diffusion, and therefore enhance tensile strength and thermal conduction of the composites. For the composites sintered at 750 °C, the density and interface bonding increase, however the Ag coating dissolves, bringing about the increase of strength, but the reduction of thermal conduction of the composites. The 50 wt% Ag(Invar)/Cu composite sintered at 700 °C has the maximum thermal conductivity (151.6 W/(m·K)) than the others of the same compositions reported so far.
科研通智能强力驱动
Strongly Powered by AbleSci AI