Yongqiang Chen,Bingbing Fan,Gang Shao,Rui Zhang
标识
DOI:10.1007/s40145-016-0202-4
摘要
Ultra-large zirconia toughened alumina (ZTA, mass ratio of Al2O3 and ZrO2 is 78:22) ceramics with eccentric circle shape were successfully sintered by microwave sintering with a multi-mode cavity at 2.45 GHz. The dimension of ZTA ceramics (green body) is 165 mm (outer diameter) × 25 mm (thickness). The optimized sintering temperature of microwave sintering is about 1500 °C for 30 min, and the total sintering time is about 4 h which is much shorter than that of conventional sintering. An auxiliary-heating insulation device was designed based on the principle of local caloric compensation to guarantee the intact sintered samples. With the increasing of sintering temperature, more and more microwave energy is absorbed within the entire sample, volumetric densification performs, and phases shift from m-ZrO2 phase to t-ZrO2 phase and cause Al2O3 grain growth.
科研通智能强力驱动
Strongly Powered by AbleSci AI