The low-cost and environmentally friendly perovskite-type oxide of Sr 1– x Ca x FeO 3-δ was proposed here as a new oxygen sorbent usable in a high-temperature pressure-swing adsorption (HT-PSA) process for oxygen production (separation) from air. The oxygen sorption/desorption properties of the Sr 1– x Ca x FeO 3-δ samples ( x = 0–1.0) were examined at 550 °C by means of thermogravimetric analysis (TGA). Among the examined samples, Sr 0.76 Ca 0.24 FeO 3-δ ( x = 0.24) was found to exhibit the largest value (7.8 cm 3 g –1 ) for the amount of reversibly sorbed/desorbed oxygen by the change in oxygen concentration between air (21 vol % O 2 ) and 5 vol % O 2 . For such an excellent oxygen sorption/desorption behavior to be verified, the oxygen content (oxygen nonstoichiometry, 3-δ) in Sr 0.76 Ca 0.24 FeO 3-δ was estimated as a function of ambient oxygen concentration. The oxygen content of Sr 0.76 Ca 0.24 FeO 3-δ was sensitive to the oxygen concentration and varied largely with its change, especially in the range of 5–21 vol % O 2 . Thus, it is expected that the large change in oxygen content can result in the large amount of reversibly sorbed/desorbed oxygen even by a small pressure-swing amplitude. Actually, the Sr 0.76 Ca 0.24 FeO 3-δ pellet sample was evaluated as an oxygen sorbent for the HT-PSA process by using a small-column apparatus. As a result, the amount of oxygen production for the Sr 0.76 Ca 0.24 FeO 3-δ pellet sample indicated 4.9 cm 3 g –1 per cycle at 600 °C. This value was approximately two times larger than that for the benchmark sample of La 0.1 Sr 0.9 Co 0.9 Fe 0.1 O 3-δ (LSCF1991).