氢脆
材料科学
脆化
氢
冶金
晶界
钝化
合金
渗透
极限抗拉强度
腐蚀
复合材料
微观结构
图层(电子)
化学
生物化学
有机化学
膜
作者
Yang Zhao,Jidong Wang,Su Feng,Lingyue Hu,Qifan Wu,Wenlong Qi,Tao Zhang,Fuhui Wang
出处
期刊:Corrosion
[NACE International]
日期:2023-11-30
卷期号:80 (1): 24-40
被引量:5
摘要
The hydrogen embrittlement susceptibility of electron beam melted Ti-6Al-4V alloy (ET) was compared with that of conventional wrought alloy (WT). Hydrogen permeation, electrochemical, and slow strain rate tensile tests as well as surface observation were conducted under a simulated sea environment. The results show that the hydrogen embrittlement susceptibility of ET is lower than that of WT, which can be attributed to the intense texture of ET with a smaller specific surface area of grain boundary, preventing hydrogen permeation. Moreover, with increasing depth of the ocean, the hydrogen embrittlement susceptibility of both ET and WT TC4 alloys increases considerably. This reduced hydrogen embrittlement resistance can be attributed to the degradation of the passivation film, accelerating the permeation flux of hydrogen.
科研通智能强力驱动
Strongly Powered by AbleSci AI