Yaohao Zhang,Sheng Wang,Liuqing Huang,Sa Zhang,Guangyu Chen,Chentong Zhang,Huaxian Cai,Jinshui Meng,Xuetao Luo
标识
DOI:10.1021/acssuschemeng.0c03875
摘要
In order to recover silicon from diamond wire sawing waste, silicon extraction and boron removal are two key issues that need to be addressed. In this study, a combined process of pressure-less sintering and CaO–SiO 2 slag treatment was proposed. Low -boron silicon was prepared and considered as raw materials in solar cell production. The results confirmed that pressure-less sintering was beneficial for the digestion of the silicon oxide layer, and the molar percentage of oxygen in silicon kerf was reduced from 14.83 to 7.24% after pressure-less sintering at 1400 °C for 2 h. The effect of slag composition on boron removal was investigated. It was found that an optimum boron removal efficiency of 86.91% was obtained when the optical basicity reached 0.68 and no CaF 2 was added; the CaO–SiO 2 mass ratio was 1.2, the holding time was 40 min, and the slag to silicon mass ratio was 1. Although the addition of CaF 2 can decrease the viscosity, it affects the activity and the oxygen potential of slag.
科研通智能强力驱动
Strongly Powered by AbleSci AI