Jie Gao,Weichang Guo,Hengrui Yang,Fei Shen,Xiaogang Han
标识
DOI:10.1007/978-981-33-6609-1_38
摘要
Garnet-type Li6.4La3Zr1.4Ta0.6O12 (LLZTO) is considered as one of the most potential electrolytes for solid state lithium batteries. Sintering process is a critical step in the preparation of LLZTO. Herein, LLZTO solid-state electrolytes were prepared by high temperature solid-phase reaction with different sintering temperature from 1150 to 1250 °C and different sintering holding time from 1 min to 60 min. According to EIS, electrolytes with high ionic conductivity up to 8.1 × 10−4 S cm−1 were obtained by sintering at 1200 °C for 20 min. Besides, LLZTO pellets prepared in this experimental condition show high density reaching up to 97.6%. Li symmetric cell with the LLZTO sintered at 1200 °C for 20 min also exhibits stable cycle performance under current density of 0.25 mA cm−2 at room temperature.
科研通智能强力驱动
Strongly Powered by AbleSci AI