Zirconia crowns exhibit significantly higher fracture resistance compared with lithium disilicate crowns, making them better suited to handle higher masticatory loads encountered in the posterior region of the mouth. Lithium disilicate can survive more than five clinical years (when their thickness is 1.1 mm).