锂(药物)
石墨
晶体结构
插层(化学)
相变
熵(时间箭头)
热力学
材料科学
电化学
磁滞
凝聚态物理
结晶学
化学
无机化学
物理
物理化学
电极
冶金
医学
内分泌学
作者
Rachid Yazami,Yvan Reynier
标识
DOI:10.1016/j.jpowsour.2005.05.087
摘要
We found anomalous behaviors during lithium electrochemical intercalation into graphite in the entropy curve and the crystal structure, especially, during the stages from 2 to 1 transition at x = 0.5 in LixC6. The entropy first decreases monotonously, then re-increased sharply at the transition. The average interlayer spacing displays a hysteresis during intercalation and de-intercalation and departs from linearity. The results are discussed in relation with a contribution of the vibrational entropy and possible occurrence of intermediary phase(s) between the two lithium-rich intercalation stages.