Necla Demir,Mehtap GÖKKAYA BOZKURT,Tuğba Temizci
标识
DOI:10.1088/2053-1591/ad524e
摘要
Abstract Objective . To compare the shear bond strength values of current CAD/CAM materials and to evaluate the color changes resulting from immersion in coloring solutions. Material and Methods . A total of 160 specimens were prepared from 4 CAD/CAM blocks; lithium disilicate glass ceramic (IPS E.max CAD[EC]), zirconia reinforced lithium silicate ceramic (Vita Suprinity[VS]), polymer infiltrated glass ceramic (Vita Enamic[VE]) and hybrid ceramic (GC Cerasmart [GC]). The ceramic specimens were immersed in tea, coffee, cherry juice and distilled water solutions. Color measurements were made. To compare the shear bond strength values, all specimens were bonded to resin cement. Then the specimens were aged with 5000 thermocycling. The failure modes were classified according to stereomicroscope analysis and than scanning electron microscopy images for surface topography were obtained. Results . The color change values were significantly greater in coffee compared to other solutions and the highest color change was seen in GC and VE. The highest bond strength values were seen in VS and VE. The shear bond strength values are listed as follows: VS>VE>EC>CS. Conclusions . EC and VS can be used, especially in aesthetic restorations, due to their high color stability. Additionally, considering the bond strength values of VS, it appears to be a highly satisfactory material.
科研通智能强力驱动
Strongly Powered by AbleSci AI