材料科学
粉末冶金
冶金
微观结构
金属间化合物
金相学
材料加工
金属粉末
复合材料
形态学(生物学)
作者
Dexin Zhang,Can Li,T.T. Zhao,Huiqiao Du,Yong Li
标识
DOI:10.1016/j.jmrt.2026.04.112
摘要
A rapid fabrication of pre-sintered TiAl alloy by spark plasma sintering with elemental powders is reported in this study. The reaction behavior between elemental powders and the effect mechanisms of sintering temperature on the microstructure and mechanical properties are systematically investigated. The results show that microstructures are mainly composed of α-Ti, γ-TiAl, α 2 -Ti 3 Al, and B2 phases, which vary in volume fraction with different sintering temperatures. The higher sintering temperature promotes the diffusion reactions between elemental powders and hence contributes to the consumption of α-Ti and the generation of particular intermetallic compounds. The average grain sizes of γ-TiAl and α 2 -Ti 3 Al phases exhibit the same trend of initially decreasing and then increasing with the increase of sintering temperature. As the sintering temperature increases from 1050 °C to 1250 °C, the density and compression strength of the alloy gradually increase. The densities of the samples all exceed 98% and reach a maximum value of 99.3% at 1250 °C. The compression property of the alloy depends on the synergistic effect of densification and microstructure, which results in a maximum compression strength of 1312 MPa with a fracture strain of 8.9% under the sintering temperature of 1250 °C. All the fracture surfaces exhibit brittle fracture features after compression tests. The relationships between the microstructures and corresponding mechanical properties are discussed in detail.
科研通智能强力驱动
Strongly Powered by AbleSci AI